Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Mechanical Lock on mould making
Mechanical Lock on mould making
Post Reply
Like
5
Mechanical Lock on mould making
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
We always recommend ensuring you have a small draught angle to the near vertical edges.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
Hanaldo
Hanaldo
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Acetone won't touch polyurethane, only polystyrene. The only option is to grind either the tooling board or the mould away until you can break one of them off. This is generally pretty hard to do without damaging both surfaces, but it is otherwise start again from scratch.
Reply
Like
5
benji
benji
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 48
Hi,
I did a mould using PU600 Density Polyurethane Model Board but end up having a mechanical lock when I tried to separate the mould from the board.
Apparently accetone can disolve the polyurethane but I was wandering if you guys have any advice?
cheers.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics