By benji - 3/18/2018 6:25:25 PM
Hi, I did a mould using PU600 Density Polyurethane Model Board but end up having a mechanical lock when I tried to separate the mould from the board. Apparently accetone can disolve the polyurethane but I was wandering if you guys have any advice? cheers.
|
By Warren (Staff) - 3/19/2018 10:29:47 AM
We always recommend ensuring you have a small draught angle to the near vertical edges.
|
|