Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Acetone won't touch polyurethane, only polystyrene. The only option is to grind either the tooling board or the mould away until you can break one of them off. This is generally pretty hard to do without damaging both surfaces, but it is otherwise start again from scratch.
|