It has been a while.. I do plan on sticking to this thread and post picture of all progress and steps I make and hopefully with your help I will have a finished roof installed on my race car in the end.
I have bought a water fan heater coil and I am about to place it in may garage roof.. That way I can raise the temperature when I need to paint or doing carbon etc.. I can´t use electric stuff for heating because it makes my house and workshop heating system turn down the heating and the rest of the house gets cold..
Mounting the hot water fan I have then fixed my work shop temp.. But after seeing pictures of exterior carbon parts being destroyed in the hot sun I am convinced I need to cure the roof in a higher temperature some how. I have no oven but I few electrical heating fans in a smaller room should get it to around 50 deg anyway.. Anyone else have any other suggestions?
I made a big order of fabric resins, mold materials and consumables from Easy composites and I am looking forward of using everything and hopefully be successful making car parts with infusion.
Back to mold making.. I got another roof.. I started leveling out dents and adding flanges. I made the long sides of the roof flat so they could be used as flanges and it also got rid of one more 90 deg angel making layup a bit easier. I also filled the front edge of the roof and the sides of the places where the roof moldings go. That way I hope the mold wont be mechanicaly locked by "negative" shapes to the roof plug.
After that I reminded myself why I hate sanding body filler.. It takes skill by experience and I have lost some of it.
Today I left the roof plug by a paint shop so it will be covered by 2k paint before making the mold.