hello

i have used the clear cast resin but now need to mix it with this glow powdr i have, which i did but you cant sand this resin nice, is there a resin that i can sand so that it is level with the channel in the wood i am filling with and polishes clear again ?

thanks
Reply
GreyArea
G
Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)
Group: Forum Members
Posts: 36, Visits: 65
It wasn’t really use of sandpaper I was thinking of...more selection of materials. For instance I didn’t realise until I read it here that one of the clear resins remains tacky if exposed rather than enclosed completely in a mould. I will check the other video out that you mentioned though.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
john arnold - 8 Years Ago
Warren (Staff) - 8 Years Ago
john arnold - 8 Years Ago
Rich (Staff) - 8 Years Ago
john arnold - 8 Years Ago
Warren (Staff) - 8 Years Ago
             ok thanks a lot ill give it a go
john arnold - 8 Years Ago
GreyArea - 8 Years Ago
Warren (Staff) - 8 Years Ago
GreyArea - 8 Years Ago
Warren (Staff) - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search