By john arnold - 2/23/2017 10:09:29 PM
hello
i have used the clear cast resin but now need to mix it with this glow powdr i have, which i did but you cant sand this resin nice, is there a resin that i can sand so that it is level with the channel in the wood i am filling with and polishes clear again ?
thanks
|
By Warren (Staff) - 12/4/2017 9:23:26 AM
As casting resins go, the only product we have that cures with a tacky finish in air is our Water Clear Polyester Casting Resin. However that is easily solved using Solution MW Wax Gelcoat Additive
|
|