resin i can sand


Author
Message
john arnold
john arnold
Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)
Group: Forum Members
Posts: 4, Visits: 10
hello

i have used the clear cast resin but now need to mix it with this glow powdr i have, which i did but you cant sand this resin nice, is there a resin that i can sand so that it is level with the channel in the wood i am filling with and polishes clear again ?

thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
john arnold - 9 Years Ago
Warren (Staff) - 9 Years Ago
john arnold - 9 Years Ago
Rich (Staff) - 9 Years Ago
john arnold - 9 Years Ago
Warren (Staff) - 9 Years Ago
             ok thanks a lot ill give it a go
john arnold - 9 Years Ago
GreyArea - 9 Years Ago
Warren (Staff) - 9 Years Ago
GreyArea - 9 Years Ago
Warren (Staff) - 9 Years Ago