Group: Forum Members
Posts: 36,
Visits: 65
|
This partly answered a question I had too. I’ve sanded cast acrylic rods (bought as solid, not cast myself) to high gloss before using 1600 grit paper after cutting. With “self cast” I’ve seen recommendations to “glaze” finished articles with a thin coat of resin (which is good advice for complex intricate surfaces) but I was wondering if that was necessary or if 1600 grit would get something like on a surface that is mostly “flat”, or at least, smooth?
Do you have any advice sheets (videos?) on how to achieve the best gloss finish with your various materials? With the range of options you have for clear finishes I’m sure a lot of your customers would find it helpful (me for one)!
|