resin i can sand


Author
Message
john arnold
john arnold
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 4, Visits: 10
hello

i have used the clear cast resin but now need to mix it with this glow powdr i have, which i did but you cant sand this resin nice, is there a resin that i can sand so that it is level with the channel in the wood i am filling with and polishes clear again ?

thanks
Reply
GreyArea
G
Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)
Group: Forum Members
Posts: 36, Visits: 65
This partly answered a question I had too. I’ve sanded cast acrylic rods (bought as solid, not cast myself) to high gloss before using 1600 grit paper after cutting. With “self cast” I’ve seen recommendations to “glaze” finished articles with a thin coat of resin (which is good advice for complex intricate surfaces) but I was wondering if that was necessary or if 1600 grit would get something like on a surface that is mostly “flat”, or at least, smooth?

Do you have any advice sheets (videos?) on how to achieve the best gloss finish with your various materials? With the range of options you have for clear finishes I’m sure a lot of your customers would find it helpful (me for one)!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
john arnold - 8 Years Ago
Warren (Staff) - 8 Years Ago
john arnold - 8 Years Ago
Rich (Staff) - 8 Years Ago
john arnold - 8 Years Ago
Warren (Staff) - 8 Years Ago
             ok thanks a lot ill give it a go
john arnold - 8 Years Ago
GreyArea - 8 Years Ago
Warren (Staff) - 8 Years Ago
GreyArea - 8 Years Ago
Warren (Staff) - 8 Years Ago