Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
resin i can sand
resin i can sand
Post Reply
Like
4
resin i can sand
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
john arnold
john arnold
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 10
hello
i have used the clear cast resin but now need to mix it with this glow powdr i have, which i did but you cant sand this resin nice, is there a resin that i can sand so that it is level with the channel in the wood i am filling with and polishes clear again ?
thanks
Reply
Like
4
Replies
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
It shouldn't cause any permanent marking on the wood itself. Any contaminants would usually wash off.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
6
john arnold
john arnold
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 10
ok thanks a lot ill give it a go
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
resin i can sand
john arnold
-
8 Years Ago
Hi John, what resin are you currently using? For filling a channel in wood, typically our GlassCast...
Warren (Staff)
-
8 Years Ago
yeah it is clear cast epoxy resin but i sanded it up to grit 220 do i need to go a lot finer thanks...
john arnold
-
8 Years Ago
Hi John. You'll need to work to much finer grades of wet/dry abrasive paper. To remove the light...
Rich (Staff)
-
8 Years Ago
ok thanks foir that but wouldn't the cutting compound affect the surrounding wood, maybe it would...
john arnold
-
8 Years Ago
It shouldn't cause any permanent marking on the wood itself. Any contaminants would usually wash...
Warren (Staff)
-
8 Years Ago
ok thanks a lot ill give it a go
john arnold
-
8 Years Ago
This partly answered a question I had too. I’ve sanded cast acrylic rods (bought as solid, not cast myself) to high gloss before using 1600 grit paper after cutting. With “self cast” I’ve seen...
GreyArea
-
8 Years Ago
We don't have any videos specifically on how to use sand paper and polish to get a smooth finish. It is covered in a couple of our other videos especially our video on How to Cover Existing Parts in...
Warren (Staff)
-
8 Years Ago
It wasn’t really use of sandpaper I was thinking of...more selection of materials. For instance I didn’t realise until I read it here that one of the clear resins remains tacky if exposed rather than...
GreyArea
-
8 Years Ago
As casting resins go, the only product we have that cures with a tacky finish in air is our Water Clear Polyester Casting Resin. However that is easily solved using Solution MW Wax Gelcoat Additive
Warren (Staff)
-
8 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search