I have rather stupidly got alot of epoxy on the Black vaccum attachment on the top of my catchpot. (the one which the infusion line goes into) I can't see it as a listed spare do you have them or can you give me a place I can buy one.

I have dissassebled the part cleaned down but can't hold a full vacumn  

Thanks
Reply
D3O Phil
D3O Phil
Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)
Group: Forum Members
Posts: 22, Visits: 498
Hi Dravis

mine didn't seemed to be glued to the lid just a nut at the bottom (just epoxy everywhere else)

One of my electricians has spotted me interwebbing and reckons it is just a regular electrical cable gland, will update if I find out