Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I think the bottom part of the black "socket" is actually glued into the lid .. like the gauge and the hose connector to the vacuum pump --
Mine ended up so covered in resin on the acrylic that I purchased the replacement lid .. I'm now in the process of refurbishing the old one with new connectors after polishing the acrylic up ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|