By D3O Phil - 6/1/2017 12:35:59 PM
I have rather stupidly got alot of epoxy on the Black vaccum attachment on the top of my catchpot. (the one which the infusion line goes into) I can't see it as a listed spare do you have them or can you give me a place I can buy one.
I have dissassebled the part cleaned down but can't hold a full vacumn
Thanks
|
By VVS - 6/4/2017 8:23:23 AM
Never had an issue with the pipe inlet, its simple and works.
If you are get loads of resin in the pot then you need to look at your infusion process, ive had the same cup in now for a year and there's about 4mm of resin in the bottom.
|
|