Group: Forum Members
Posts: 73,
Visits: 473
|
I want to make a 2-part mould roughly covering 3.5sqmtrs but the overall cost is quite large.
Would it be possible to use a cheaper alternative to the Uni-mould Tooling resin (which appears to be the most expensive part) such as a cheap Polyester resin to bond all the layers of chopped strand mat? Or is there another cheaper alternative to the uni-mould system that would give adequate results?
I don't intend on pulling hundreds of releases, at most I would say 5 in total?
|