What resin on existing parts ... Poliester or Epoxy ?
What resin on existing parts ... Poliester or Epoxy ?
Post Reply
Like
3
What resin on existing parts ... Poliester or Epoxy ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
fibernoob
fibernoob
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 34,
Visits: 134
Hey all.
When having to repair an existing part what is the best way to find out what resin the part is made of?
Is there a simple method to detect the poliéster or epoxy?
I have been told to burn the resin and detect the color of the smoke (black = poliester , colourless = epoxy).
This obviously is not a very practical method with existing parts that need repair.
Thanks in advance.
Reply
Like
3
Reply
fibernoob
fibernoob
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 134
Thank-you ....
Will start sniffing ...
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
What resin on existing parts ... Poliester or Epoxy ?
fibernoob
-
8 Years Ago
If you can see any CSM (chop strand matt) then it is likely polyester or vinylester. If you know...
Fasta
-
8 Years Ago
Thank-you .... Will start sniffing ... :P
fibernoob
-
8 Years Ago
In all honesty, I don't believe it matters too much. Epoxy has the highest bond strength of the...
Hanaldo
-
8 Years Ago
"epoxy doesn't stick to polyester" Thanks again Hanaldo .... its exactly that statement that was...
fibernoob
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search