Hey all.
When having to repair an existing part what is the best way to find out what resin the part is made of?
Is there a simple method to detect the poliéster or epoxy?
I have been told to burn the resin and detect the color of the smoke (black = poliester , colourless = epoxy).
This obviously is not a very practical method with existing parts that need repair.
Thanks in advance.