Hey all. 

When having to repair an existing part what is the best way to find out what resin the part is made of?



Is there a simple method to detect the poliéster or epoxy? 





I have been told to burn the resin and detect the color of the smoke (black = poliester ,  colourless = epoxy).

This obviously is not a very practical method with existing parts that need repair.



Thanks in advance.
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
If you can see any CSM (chop strand matt) then it is likely polyester or vinylester. If you know what these materials smell like then just give it a slight sanding and take a sniff.

The polyester/vinylester will have a noticable smell whereas an epoxy laminate does not really have a strong scent of anything.




Edited 8 Years Ago by Fasta
fibernoob
fibernoob
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Thank-you ....  

Will start sniffing ... Tongue
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
In all honesty, I don't believe it matters too much. Epoxy has the highest bond strength of the three resins, and so is the natural choice for a repair on an unknown laminate. 

If you are being put off by the statement that epoxy doesn't stick to polyester, then don't be. I have done hundreds of repairs epoxy resin on polyester parts, none of them have failed due to delamination. I suspect the statement has more to do with trying to bond epoxy to a freshly produced polyester laminate with minimal surface prep, in which case I could understand a poor bond. But on a properly cured laminate with a well keyed/cleaned surface, epoxy will stick like the proverbial. 
fibernoob
fibernoob
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 34, Visits: 134
"epoxy doesn't stick to polyester"



Thanks again Hanaldo .... its exactly that statement that was getting to me.... Had it as a golden rule from all the theory ...
Edited 8 Years Ago by fibernoob
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search