What resin on existing parts ... Poliester or Epoxy ?
What resin on existing parts ... Poliester or Epoxy ?
Post Reply
Like
3
What resin on existing parts ... Poliester or Epoxy ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
fibernoob
fibernoob
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 34,
Visits: 134
Hey all.
When having to repair an existing part what is the best way to find out what resin the part is made of?
Is there a simple method to detect the poliéster or epoxy?
I have been told to burn the resin and detect the color of the smoke (black = poliester , colourless = epoxy).
This obviously is not a very practical method with existing parts that need repair.
Thanks in advance.
Reply
Like
3
Fasta
Fasta
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
If you can see any CSM (chop strand matt) then it is likely polyester or vinylester. If you know what these materials smell like then just give it a slight sanding and take a sniff.
The polyester/vinylester will have a noticable smell whereas an epoxy laminate does not really have a strong scent of anything.
Fastacraft Facebook page
Edited
8 Years Ago by
Fasta
Reply
Like
2
fibernoob
fibernoob
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 134
Thank-you ....
Will start sniffing ...
Reply
Like
3
Hanaldo
Hanaldo
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
In all honesty, I don't believe it matters too much. Epoxy has the highest bond strength of the three resins, and so is the natural choice for a repair on an unknown laminate.
If you are being put off by the statement that epoxy doesn't stick to polyester, then don't be. I have done hundreds of repairs epoxy resin on polyester parts, none of them have failed due to delamination. I suspect the statement has more to do with trying to bond epoxy to a freshly produced polyester laminate with minimal surface prep, in which case I could understand a poor bond. But on a properly cured laminate with a well keyed/cleaned surface, epoxy will stick like the proverbial.
Reply
Like
2
fibernoob
fibernoob
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 134
"epoxy doesn't stick to polyester"
Thanks again Hanaldo .... its exactly that statement that was getting to me.... Had it as a golden rule from all the theory ...
Edited
8 Years Ago by
fibernoob
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search