Hi 

I'm from belgium 
We have order in few moth different consumable to made a hood in infusion 

the finish is good, i have 100% vacuum, we use the resin IN2 epoxy, all it's good but we have place the soric2 and 3 in different part's to test the resistant finish and i have this propleme > show this picture  



I have test the infusion with 1,2 and 3 layer and i have always this mark in the carbon 

The cure cycle is respect, the vacuum is full it's your resin 

I don't enderstant were is the problem 
I your tutorial with the hood for the mini the technician use only 1 layer carbon and direct the soric2 

Have you a idea why i have this mark ? 

Thanks in advance 
Devillers Cedric 
FC Design manager 
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi,

Have you used carbon tape to build the thickness at the edges to match the soric? In the Bonnet video we used to tape to match the thickness so that there is no difference. If there is a difference, then usually it shows up on the surface of the finished part.  You can sand the foam to a taper to help but this is not so easy to sand soric in that fashion when compared to PVC foams.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search