Hi,
Have you used carbon tape to build the thickness at the edges to match the soric? In the Bonnet video we used to tape to match the thickness so that there is no difference. If there is a difference, then usually it shows up on the surface of the finished part. You can sand the foam to a taper to help but this is not so easy to sand soric in that fashion when compared to PVC foams.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|