Group: Forum Members
Posts: 460,
Visits: 5.2K
|
it sounds as though you have bridging in the area of the radius/contour. are you properly placing the material into the corner and using plenty of vaccum bag in the tricky areas to ensure no bridging and decent consolidation? I would look at your bagging process as the release agent will only affect your surface if its not applied properly, i the parts are being demoulded ok then its not a problem
|