Currently i have issue with surface finish of my parts. The surface has so many pinhole and also dry. Im using pre preg and autoclave cure. Does release agent play important roll in this matter .? Im also using surface master 905 , which suppose to help me improve the surface finish. 
As my mould has a contour, this defect appears along the radius of the parts contour. The flat surface is good.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search