Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Shiny on both sides
Shiny on both sides
Post Reply
Like
3
Prev
1
2
Jump To Page
Shiny on both sides
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
mannime
mannime
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 31
Hi Matthieu,
thanks for sharing that video. I'm really interested in your test results. Do you mind sharing them?
Thanks
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Well I did this for personal use, to add to my "material library" I haven't tested them in a lab or something like that so I don't have numbers about their stiffness and strenght.
What I can say is that the PVC foam cored sample is quit strong in ratio to his weight.
A second remarkable thing was the carbonfiber sandwich with fiberglass. I've did Carbon-glas-Carbon-glas-Carbon resulting in a very stiff, but heavier part.
samples with the carbon only start to get stiff after 5+ layers. When there are less layers its quit easy to bend.
I'll try to upload a new video talking about the weight and more details on the samples in the near future
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search