I made a unimold of a plug today. The plug got bad and also the mold. Does anyone know what can have caused these problems? I have use both the pattern coat primer and the hi gloss on a MDF pattern. 


Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Looks like a release problem. I assume you are using Easylease? How did you apply it, how old is it? 

Often stress cracks like this are caused when there is a partial release failure, so it hasn't completely stuck but it takes too much force to demould. The bits of stuck gelcoat also tell me this was the case. 