Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
Plug issues
Plug issues
Post Reply
Like
3
Plug issues
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ArturK
ArturK
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 19,
Visits: 53
The problem can be:
1. Temperature at your workplace (most separators needs >25 C temperature during application)
2. Mould coating - do not know this products, but many standards coats react with release agents. Mould coating has to be fully cured of course (some products needs even 14 days after coating for full curing.
3. Release agent itself.
Carbon fiber sheets and composites .
www.dexcraft.com
Reply
Like
4
VVS
VVS
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
i always leave the metal seal in the tin and make a small hole in one side so you only get a trickle coming out.
Reply
Like
4
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
It sounds like this was definitely a release failure. How well did you clean the plug before applying it, did you use a solvent?
How well sealed have you kept the bottle of Easylease? When you are applying it, do you keep the lid off or do you put the lid back on straight away before applying it to the mould?
Chemical release agents are very sensitive to moisture and are hygroscopic by nature, so you need to be quite careful with how well sealed you keep the bottle and how often you expose it to the air.
Reply
Like
4
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 486
Yes I used a 8 month old easy lease. Applyed it with a cloth six times like I always do. 15 minutes between each and 1 hour before first layer of gel coat. Yes i had some trouble releasing it.
Reply
Like
4
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Looks like a release problem. I assume you are using Easylease? How did you apply it, how old is it?
Often stress cracks like this are caused when there is a partial release failure, so it hasn't completely stuck but it takes too much force to demould. The bits of stuck gelcoat also tell me this was the case.
Reply
Like
3
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I made a unimold of a plug today. The plug got bad and also the mold. Does anyone know what can have caused these problems? I have use both the pattern coat primer and the hi gloss on a MDF pattern.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search