			            You seem to be making things very difficult for yourself when you bag up 
  Put the sealing tape on the bag before you put the part in,open the bag up and press the tape onto the bag laying nice flat an smooth on the table
  tape right on the edge of the bag and use the edge as a guide,lot earier when you came to seal an you can see the join right on the edge of the job and not having 6" of bag in the way                
			            				
			                                 
                     
                                            
                         
                    
                  
             |