Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Body Package for Dax Rush with Side Intrusion Bars
Body Package for Dax Rush with Side Intrusion Bars
Post Reply
Like
13
1
2
3
4
5
14
Next
Jump To Page
Body Package for Dax Rush with Side Intrusion Bars
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
davro
davro
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
A couple of images of the aero screen installed just needs a small bead of black silicon to bond it to the scuttle.
Have started a new job so most of my time is taken up with this now.
But winter is coming and I do have some winter project upgrades planned while the car is off the road.
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
9 Years Ago by
davro
Reply
Like
6
davro
davro
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Test fitting the new Aeroscreen, just need to finish fitting sanding edges to shape, drill some fixing holes :/ and then get it 2K clear coated for some UV protection and the weight so far is 450 grams.
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
9 Years Ago by
davro
Reply
Like
6
davro
davro
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Reply
Like
7
davro
davro
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Nearly ready to layup and do an infusion
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Reply
Like
6
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
OliilO (22/11/2016)
What do you use to polish your moulds prior to their first use?
I've just taken a mould from one of my cycle wings and have been pleased with how it came out so far. I feel giving it a quick polish would help improve the quality of the finished product even though visually the mould looks good now.
Do yourself a favour and give the Pai Crystal range from Easy Composites a go! The NW1 cutting compound is far and above the best compound I have ever used, and I've used a lot! That on its own will give you a very good gloss, but I also always use the Easy Gloss Black which is the second stage in the system. It's magic stuff.
Reply
Like
5
OliilO
OliilO
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 126
What do you use to polish your moulds prior to their first use?
I've just taken a mould from one of my cycle wings and have been pleased with how it came out so far. I feel giving it a quick polish would help improve the quality of the finished product even though visually the mould looks good now.
Reply
Like
6
davro
davro
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
The Dax Rush MC, Modified Aeroscreen mould separated from the pattern nicely
Just need to trim the edges and give it a polishing before making some carbon fibre aero screens.
Looking forward to see your aeroscreen
scottracing
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
10 Years Ago by
davro
Reply
Like
6
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Good work again mate. I have a half finished aeroscreen in the garage. Hopefully i can show you some progress in the new year.
Reply
Like
11
davro
davro
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
This is an Aeroscreen mould that wraps down the side of the scuttle with some nice big flanges, that I plan on connecting to some (aero) doors eventually. I used the old scuttle as the former for the new extended Aeroscreen,
Duncan Cowper
with the insane turbo hayabusa Dax Rush gave me the original Aeroscreen that I extended
AutoGlym Hyper Fresh helps keep the smell down.
Hopefully, I should get the Aeroscreen of the composite table tomorrow, so I can start working on the rear arches again (drivers side arch to do
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
10 Years Ago by
davro
Reply
Like
7
davro
davro
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Cheers
scottracing
, looking forward to making these in carbon next, and some nice long tubes of different sizes for the intakes and then a carbon plenum no doubt
Not sure who originally machined these moulds, I did try to mill some intakes but my milling machine was just a bit too small for the job.
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
10 Years Ago by
davro
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
13
1
2
3
4
5
14
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search