Group: Forum Members
Posts: 338,
Visits: 2K
|
Having had a look at the SHD PDF, it certainly does look like it offers the opportunity for some short cure cycles, down to 3 hours for temperatures within the range of the Unimould tooling system
morepower - Is DF212 just the surface layer fabric and does it need to be backed up with another of their products, or does it come in various weights? Also, how does it stack up in terms of price when compared with EC's OOA fabric?
Realistically, will it also take fair bit of experimentation in order to achieve perfect surface finish results using this, assuming that the user has an oven with stable temperature control and the ability to ramp appropriately
Certainly looks appealing, but would just like to fully understand any 'cons' to trying it, as opposed to EC's material and I'm sure that you're well placed to make a realistic assessment of that
Cheers
Mark
|