Ive had nothing but problems with uni mould, I'm clearly doing some thing wrong haha.

Any way i pulled a part today (first time using the mould) (and first 2 piece mould) And as you can see from the pics it has gone dull and can see some print on it.

Before i layed up, the mould was really shiny.

Any advice would be great..





This is the other half (not as bad) 


Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Have you used it before? 
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
No, its the first time using the mould and easy lease
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
VVS - 10 Years Ago
Darren - 10 Years Ago
matthieutje65 - 10 Years Ago
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
TomDesign - 10 Years Ago
Rich (Staff) - 10 Years Ago
Darren - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search