Ive had nothing but problems with uni mould, I'm clearly doing some thing wrong haha.

Any way i pulled a part today (first time using the mould) (and first 2 piece mould) And as you can see from the pics it has gone dull and can see some print on it.

Before i layed up, the mould was really shiny.

Any advice would be great..





This is the other half (not as bad) 


Replies
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
As said it looks like not enough release applied.

I don't do the 4 or 5 coat thing, I apply coats until you get that feel of silk, on the 4th,5th,6th coat what ever it takes you suddenly feel a difference in how the release agent feels when applied, all goes super smooth and has a feel all of its own that it didn't have before.
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
VVS (18/10/2015)
As said it looks like not enough release applied.

I don't do the 4 or 5 coat thing, I apply coats until you get that feel of silk, on the 4th,5th,6th coat what ever it takes you suddenly feel a difference in how the release agent feels when applied, all goes super smooth and has a feel all of its own that it didn't have before.


I shall give that ago..

How long do you wait between applying coats? 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Not sure but looks like you have some print through from the heavy fiberglass cloth behind... 
So might be you haven't let the gelcoat cure enough.
Second possible problem might be how the release agent was applied, did you buff it inbetween the coats?
Have you cleaned your mould with some hot soapy water after?!

a third cause might be humidity or a bad cure due to low temperatures now

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
matthieutje65 (18/10/2015)
Not sure but looks like you have some print through from the heavy fiberglass cloth behind... 
So might be you haven't let the gelcoat cure enough.
Second possible problem might be how the release agent was applied, did you buff it inbetween the coats?
Have you cleaned your mould with some hot soapy water after?!
a third cause might be humidity or a bad cure due to low temperatures now


The print through does look like the heavy fiberglass, i mave have applied the tooling resin to early on to the coupling coat…

I didn't buff the easy lease inbertween coats, just applied with one cloth and wiped away with another

No i haven't cleaned the moulds yet
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
VVS - 10 Years Ago
Darren - 10 Years Ago
matthieutje65 - 10 Years Ago
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
Hanaldo - 10 Years Ago
Darren - 10 Years Ago
TomDesign - 10 Years Ago
Rich (Staff) - 10 Years Ago
Darren - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search