By Darren - 10/17/2015 8:42:50 PM

Ive had nothing but problems with uni mould, I'm clearly doing some thing wrong haha.

Any way i pulled a part today (first time using the mould) (and first 2 piece mould) And as you can see from the pics it has gone dull and can see some print on it.

Before i layed up, the mould was really shiny.

Any advice would be great..





This is the other half (not as bad) 

By Darren - 10/22/2015 7:56:59 PM

It didn't bead up or streak, the surface of the mould just looked wet.

I shall give it ago with putting it in on thinner and not wipe away the residue