I tried repairing my mould last night as there were a few pin holes in the surface.

I therefore mixed up some tooling gelocat and wax additive and just filled in the holes.

Its now almost 24 hours since and the repair areas are still a little tacky.

I did use the correct ratio, but obviously something hasn't gone to process.

Therefore, what is the best solution to fix this ?

Do I wipe away the existing tacky repair and try and fill them again, or is there anything you can do to harden the existing repairs ?
Replies
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Give it some heat first,see if that kicks off the cure.
Lenny
Lenny
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 16, Visits: 58
Would you suggest a heat gun over the surface for a period of time ?

I'm not entirely sure how long the repair should take to cure anyway, assumed 24 hours in ambient temp would be sufficient.