macsddau1
macsddau1
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 4,
Visits: 76
Hi,
For my first project, I want to make box for my daughter treble (she's got 3). I know how careful teenagers are...
I design the first box with 4 parts. Here are some views :
Bottom external part :
Top external part :
The internal parts :
The external dimension are 110 x 240mm.
Did you see some difficulties to make this parts with 200gsm carbon fibre 2/2 Twill, 4 plies with epoxy infusion ?
Best regards,
Denis
note : please, be indulgent of my English writing. I''m not as so fast to read and write because I have to translate to French to understand words. In your answers, could you please use common words and not local expression. In advance, thanks a lot.
Tags
Box
Music
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Musical instrument box
macsddau1
-
11 Years Ago
These are quite small boxes.. I would go for a lighter fabric than 200 gsm twill. 4 layers of 200...
Dravis
-
11 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search