These are quite small boxes.. I would go for a lighter fabric than 200 gsm twill.

4 layers of 200 gsm twill will produce a 0,8 - 1 mm thick shell, which will be much stronger than you need for these small cases.

Also a lighter weight fabric may be easier to get to conform to the small cornes and radii you have.

The inside parts with the cutouts for the instrument itself will be very difficult to get carbon fibre fabrics to conform to.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 11 Years Ago by Dravis
macsddau1
macsddau1
Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)
Group: Awaiting Activation
Posts: 4, Visits: 76
Hi,

For my first project, I want to make box for my daughter treble (she's got 3). I know how careful teenagers are...

I design the first box with 4 parts. Here are some views :
http://www.talkcomposites.com/Uploads/Images/4174249d-0d71-4709-925f-8247.jpg
Bottom external part :
http://www.talkcomposites.com/Uploads/Images/8325d20b-dafe-40c0-9145-586c.jpghttp://www.talkcomposites.com/Uploads/Images/d610643e-0848-4030-a7a9-5704.jpg
Top external part :
http://www.talkcomposites.com/Uploads/Images/b3ab3321-a7f9-456d-b78b-ed06.jpghttp://www.talkcomposites.com/Uploads/Images/7aa7c4c9-7d50-4043-bd3d-6585.jpg
The internal parts :
http://www.talkcomposites.com/Uploads/Images/c134dcb2-097c-4f4d-bd34-baa2.jpghttp://www.talkcomposites.com/Uploads/Images/53de79c7-448e-4636-845f-9bdf.jpg
The external dimension are 110 x 240mm.

Did you see some difficulties to make this parts with 200gsm carbon fibre 2/2 Twill, 4 plies with epoxy infusion ?

Best regards,

Denis

note : please, be indulgent of my English writing. I''m not as so fast to read and write because I have to translate to French to understand words. In your answers, could you please use common words and not local expression. In advance, thanks a lot.
Tags
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search