Hi,

For my first project, I want to make box for my daughter treble (she's got 3). I know how careful teenagers are...

I design the first box with 4 parts. Here are some views :
http://www.talkcomposites.com/Uploads/Images/4174249d-0d71-4709-925f-8247.jpg
Bottom external part :
http://www.talkcomposites.com/Uploads/Images/8325d20b-dafe-40c0-9145-586c.jpghttp://www.talkcomposites.com/Uploads/Images/d610643e-0848-4030-a7a9-5704.jpg
Top external part :
http://www.talkcomposites.com/Uploads/Images/b3ab3321-a7f9-456d-b78b-ed06.jpghttp://www.talkcomposites.com/Uploads/Images/7aa7c4c9-7d50-4043-bd3d-6585.jpg
The internal parts :
http://www.talkcomposites.com/Uploads/Images/c134dcb2-097c-4f4d-bd34-baa2.jpghttp://www.talkcomposites.com/Uploads/Images/53de79c7-448e-4636-845f-9bdf.jpg
The external dimension are 110 x 240mm.

Did you see some difficulties to make this parts with 200gsm carbon fibre 2/2 Twill, 4 plies with epoxy infusion ?

Best regards,

Denis

note : please, be indulgent of my English writing. I''m not as so fast to read and write because I have to translate to French to understand words. In your answers, could you please use common words and not local expression. In advance, thanks a lot.
Tags
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search