Hello Guys

Can anyone recomend a spray tack for epoxy resin infusion ?

I Infused a part on the weekend using Infuzene and it left stringy marks on the surface. Maybe i used to much but it sprays so inconsistently , hard to get only a mist.

I live in Australia so any local help with suppliers would be great.

Thanks

Rod.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh Elite are undergoing a merger at the moment, so a lot of their stuff isn't on the website at the moment. Give them a call or send Phill an email and see if they've got any in stock that they are trying to clear. 

Gotta say, I'm not a fan of Kinetix R118, it's awful epoxy. Works well as an infusion resin, but it's properties are pretty poor and it's clarity is sub-par. It's also got horrific UV resistance. For the price you pay, ATL can keep it. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
MarkMK - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
ChrisR - 10 Years Ago
rallyfly - 10 Years Ago
Warren (Staff) - 10 Years Ago
Chris Scott - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search