I sent Elite composites an email yesterday , no reply yet.   I know he is a busy man. Will try call today.

What Infusion epoxy have you found Hanaldo ?  I build Rally fairings kits for dirt bikes , everythig is painted so UV stability isnt really an issue. I have found the Kinetix

infused nicely but something that does the same job but is cheaper would interest me.
Attachments
690almostthere_zpsaac63a07.jpg (807 views, 165.00 KB)
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh Elite are undergoing a merger at the moment, so a lot of their stuff isn't on the website at the moment. Give them a call or send Phill an email and see if they've got any in stock that they are trying to clear. 

Gotta say, I'm not a fan of Kinetix R118, it's awful epoxy. Works well as an infusion resin, but it's properties are pretty poor and it's clarity is sub-par. It's also got horrific UV resistance. For the price you pay, ATL can keep it. 
rallyfly
rallyfly
Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)
Group: Forum Members
Posts: 25, Visits: 85
Thanks Hanaldo.  Im using Kinetix R118 infusion resin.

Elite dont seem to have that listed anymore on there website ?

I will call direct and ask.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Elite Composites sell Aerofix 3. Works well with the epoxy system I am using, but members from here have said it doesn't work well with the Easy Composites IN2 resin. So it does depend what resin system you are using. 
Edited 10 Years Ago by Hanaldo
rallyfly
rallyfly
Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)
Group: Forum Members
Posts: 25, Visits: 85
Hello Guys

Can anyone recomend a spray tack for epoxy resin infusion ?

I Infused a part on the weekend using Infuzene and it left stringy marks on the surface. Maybe i used to much but it sprays so inconsistently , hard to get only a mist.

I live in Australia so any local help with suppliers would be great.

Thanks

Rod.