rallyfly
rallyfly
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 25,
Visits: 85
I sent Elite composites an email yesterday , no reply yet. I know he is a busy man. Will try call today.
What Infusion epoxy have you found Hanaldo ? I build Rally fairings kits for dirt bikes , everythig is painted so UV stability isnt really an issue. I have found the Kinetix
infused nicely but something that does the same job but is cheaper would interest me.
Attachments
690almostthere_zpsaac63a07.jpg
(
808 views,
165.00 KB
)
Reply
Like
2
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yeh Elite are undergoing a merger at the moment, so a lot of their stuff isn't on the website at the moment. Give them a call or send Phill an email and see if they've got any in stock that they are trying to clear.
Gotta say, I'm not a fan of Kinetix R118, it's awful epoxy. Works well as an infusion resin, but it's properties are pretty poor and it's clarity is sub-par. It's also got horrific UV resistance. For the price you pay, ATL can keep it.
Reply
Like
2
rallyfly
rallyfly
posted 10 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 25,
Visits: 85
Thanks Hanaldo. Im using Kinetix R118 infusion resin.
Elite dont seem to have that listed anymore on there website ?
I will call direct and ask.
Reply
Like
1
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Elite Composites sell Aerofix 3. Works well with the epoxy system I am using, but members from here have said it doesn't work well with the Easy Composites IN2 resin. So it does depend what resin system you are using.
Edited
10 Years Ago by
Hanaldo
Reply
Like
2
rallyfly
rallyfly
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 25,
Visits: 85
Hello Guys
Can anyone recomend a spray tack for epoxy resin infusion ?
I Infused a part on the weekend using Infuzene and it left stringy marks on the surface. Maybe i used to much but it sprays so inconsistently , hard to get only a mist.
I live in Australia so any local help with suppliers would be great.
Thanks
Rod.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search