Use carbon fiber part to fix/reinforce ABS parts


Author
Message
ducatichiang
ducatichiang
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 2, Visits: 29
Hi everyone,

Sorry for my poor English.

I want to use carbon fiber to fix/reinforce my scooter ABS parts.
The plan is make some carbon fiber tenon(Sorry. I am not sure how to call it in English...) to replace original tenon on the part.
Please refer to the red mark in the picture.
http://www.talkcomposites.com/Uploads/Images/5b903cdb-2b2f-4b7b-8c92-44c9.JPGhttp://www.talkcomposites.com/Uploads/Images/2a0fd6f5-4bc5-4735-9bdd-041f.jpg

I need make two materials stick together(ABS and carbon fiber).
The question is what kind of adhesive should I use?
E515, ET500, ET538,  PT326, PU18  or others solution/advised?

Best Regards & Thanks
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Chris is correct with the preparation and epoxy will bond when used in this way.

However we would recommend our VuduGlu™ VM100 Black as it has a slightly better bond strength when used on hard to bond to plastics such as ABS.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search