Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
Use carbon fiber part to fix/reinforce ABS parts
http://www.talkcomposites.com/Topic18138.aspx
By ducatichiang
-
6/11/2015 7:44:11 PM
Hi everyone,
Sorry for my poor English.
I want to use carbon fiber to fix/reinforce my scooter ABS parts.
The plan is make some carbon fiber tenon(Sorry. I am not sure how to call it in English...) to replace original
tenon on the
part.
Please refer to the red mark in the picture.
I need make two materials stick together(ABS and carbon fiber).
The question is what kind of adhesive should I use?
E515, ET500, ET538, PT326, PU18 or others solution/advised?
Best Regards & Thanks
By ducatichiang
-
6/14/2015 3:59:55 AM
Thank you all of you!!
These information are very useful and important to me.
Best Regards & Thanks