Darren
Darren
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 54,
Visits: 916
Another update.
Slowly getting there now..
Made the controller box, this will also have the ssr inside
Switches in
Fan motor mounted
Reply
Like
4
AlessandroPA
AlessandroPA
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 301
Welll done! I can't wait to see the oven when completed
Darren (20/05/2015)
Thanks for the comments guys.
Haven't had much time on this so only a small update…
Got the fan mount welded in
Also got my pid controller and ssr through the post today
Reply
Like
5
Darren
Darren
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 54,
Visits: 916
Thanks for the comments guys.
Haven't had much time on this so only a small update…
Got the fan mount welded in
Also got my pid controller and ssr through the post today
Reply
Like
4
AlessandroPA
AlessandroPA
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 301
It looks nice! I will keep an eye to understand how to build an oven for me
Reply
Like
5
wojtepanik
wojtepanik
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
looks badass !! keep us informing !
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
6
Shaneer22
Shaneer22
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 156,
Visits: 14K
Any more progress.
Reply
Like
6
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
I would also recommend VacInnovations, they have all the kit you could possibly need and whenever I have rung them they have been helpful.
Reply
Like
6
f1rob
f1rob
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
Vac innovations
Reply
Like
5
Darren
Darren
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 54,
Visits: 916
davro (01/05/2015)
Looking good so far! are you going to have any runners for shelves inside the oven.
I am about to start building my oven in the next week or so
I'm just going to have one fixed shelf in it.
Any body know a good place to buy vac fittings?
Reply
Like
5
davro
davro
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Looking good so far! are you going to have any runners for shelves inside the oven.
I am about to start building my oven in the next week or so
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
11 Years Ago by
davro
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Prev
1
2
3
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search