By Darren
-
4/29/2015 4:33:36 PM
Started an oven build today so thought i would make a thread to post my progress.
This is all new to me so I'm sure il have some questions on the way, and you can all correct me if i do something wrong
Made the frame out of 15mm steel box tube
Then a 1mm steel outer skin
What size element would be good for this size oven?
Its 1 meter x 600mm x 600mm
By 67redrocket
-
3/29/2016 12:33:41 PM
Hello, Iam also lookingat building a oven, what type of heater/fan is that?