Ok here is a question, I would like to know if it is possible to lay (4) small molds is a casting box, using the resin infusion process for a parts run, end result (4) parts ready for finishing.

Now take in consideration that everything is done properly, gel coating, bagging, correct amount of resin etc.

could you elaborate please.
Reply
Carbon Tuner
Carbon Tuner
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 104, Visits: 422
If my opinion is worth anything I'd say you sure could. Just need to get a few of those resin injection rubber grommets and make a make a equal amount of resin flow tube to each part, "branch it out”.

I had thought about this but decided against it, though about making a 4 partmould of the same part "small". it’s just more risk for not much reason. Why not just make 4 molds instead of one big one? that way if you break the mould your only down 1 not all 4. also if something goes wrong you need to abort mission on all with a single mold.

Plus getting the bagging material to lay on 4 could end up being a challenge for me!





If Brute Force Isn''''t working your not using enough...
Edited 13 Years Ago by Carbon Tuner
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search