Bloody good work!
Some people keep the pump on all the time anyway, so if it can hold a vacuum despite the leak, as you found youd get away with it to an extent.
If youve got any pinholes in the areas you want visible, then fill them with resin. I presume the whole thing will be laquered on top of the paint and bare carbon anyway? If so you should be able to repair any pinholes and they will be virtually impossible to see once lacquered and fitted to car.
Fantastic weight saving too. I imagine you could pretty much to the whole body in CF and have a really light weight noble.
Just take your time with trimming and finishing off. Youve come too far to screw it up by rushing it!!
|