Hi guys,

I use Carbon, E glass, S glass, Kevlar types of fibers with different areas and thicknesses. Sometimes we had a big problem because stirred too much resin and hardener. Then I researched and find something useful for me from Gurit,Easycomposites and my supervisor Dr. Icten. I wrote an application for android phones. You can download with this link to your android phone.

Here is video; 

http://youtu.be/AyyDMpZlF70

Don't forget this is only for infusion process. Notakes responsibility for mistakes. It is compatible with laminates, is not for sandwich composites because core materials absorb different amount of resin.

What do youthink about my app, please share with me your ideas, offer for this.

Thanks guysJ



Edited 10 Years Ago by erdemy1
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I have played with the app and compared it to our Resin Usage Calculator and found the figures are within a few percent in most cases which is more than close enough considering different views on "wastage levels" and peel ply uptakes etc.

I think it may be possible to add cores to it.  You would need an extra figure in the calculation - resin uptake in g/m2.  Some of the cores have that data available and it can be calculated for others by back calculating weight of the part with known laminate in it.

Resin ratio calculator seems to work fine from a few quick checks Ive done.

Looks to me like it will save people time so gets the thumbs up from me.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search