erdemy1
erdemy1
Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)
Group: Forum Members
Posts: 11, Visits: 225

Hi guys,

I use Carbon, E glass, S glass, Kevlar types of fibers with different areas and thicknesses. Sometimes we had a big problem because stirred too much resin and hardener. Then I researched and find something useful for me from Gurit,Easycomposites and my supervisor Dr. Icten. I wrote an application for android phones. You can download with this link to your android phone.

Here is video; 

http://youtu.be/AyyDMpZlF70

Don't forget this is only for infusion process. Notakes responsibility for mistakes. It is compatible with laminates, is not for sandwich composites because core materials absorb different amount of resin.

What do youthink about my app, please share with me your ideas, offer for this.

Thanks guysJ



Edited 10 Years Ago by erdemy1
Reply
erdemy1
erdemy1
Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)
Group: Forum Members
Posts: 11, Visits: 225
hi Matt,
Firstly, my ratio is 60/40 which i tried with small to large productions i.e. 0,45 m^2, 45 layers, 600 g/m^2 glass fiber; 10 m^2, 2 layers 300 g/m^2 carbon fiber, 1,12 m^2 28 layers 300 g/m^2 glass fiber etc.
I added peel ply, infusion mesh and pipes.  
This program for gives an ideas for your infusion, it is not possible get directly right weight.
I think it is normal for very small infusions.
Thanks for your comments Smile  

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search