I have been working with carbon fiber since this year so I'm still a rookie I would say. I doing some CF myself and I'm wondering if I could use pre preg to do laminations of the nterior trim ?
Drew Diller
Drew Diller
Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)
Group: Forum Members
Posts: 35, Visits: 199
Interior trim of what? It is unclear what you wish to make.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
It is possible but keep in mind you'll need an oven and vacuum supply resistent till high temperatures and an oven Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




TomRiddel
TomRiddel
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 15
Drew Diller (04/07/2014)
Interior trim of what? It is unclear what you wish to make.


Of an 335i bmw. I just want to know how to do lamination with pre preg ...
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
i think do not try as your plastic gonna be deformated and melted. so better try hands wrap.
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I have tried this. Sometimes it works and most times it does not.

The main issue is that the plastics expand a lot with heat, when the plastic parts have different thickness they expand different amounts so this will bend and change the shape of your parts.




Edited 11 Years Ago by Fasta
TomRiddel
TomRiddel
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 15
So manufacturing the part from pre preg would be the best idea ?
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Best idea if you're just wanting the cosmetics is to wrap the part wet lay style