Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
Could I do this ?
Could I do this ?
Post Reply
Like
3
Could I do this ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomRiddel
TomRiddel
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 15
I have been working with carbon fiber since this year so I'm still a rookie I would say. I doing some CF myself and I'm wondering if I could use pre preg to do laminations of the nterior trim ?
Reply
Like
3
Reply
TomRiddel
TomRiddel
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 15
Drew Diller (04/07/2014)
Interior trim of what? It is unclear what you wish to make.
Of an 335i bmw. I just want to know how to do lamination with pre preg ...
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Could I do this ?
TomRiddel
-
11 Years Ago
Interior trim of what? It is unclear what you wish to make.
Drew Diller
-
11 Years Ago
It is possible but keep in mind you'll need an oven and vacuum supply resistent till high...
matthieutje65
-
11 Years Ago
[quote][b]Drew Diller (04/07/2014)[/b][hr]Interior trim of what? It is unclear what you wish to...
TomRiddel
-
11 Years Ago
i think do not try as your plastic gonna be deformated and melted. so better try hands wrap.
TomDesign
-
11 Years Ago
I have tried this. Sometimes it works and most times it does not. The main issue is that the...
Fasta
-
11 Years Ago
So manufacturing the part from pre preg would be the best idea ?
TomRiddel
-
11 Years Ago
Best idea if you're just wanting the cosmetics is to wrap the part wet lay style
ajb100
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search