Front Splitter


Author
Message
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
The Fiesta St I have been making parts for doesn't have a splitter as standard, this one I made should be fitted to the car pretty soon. Lay up was  GC 50 - 2 x 450 CF - 10mm foam core - 2 x 450 CF using infusion.

Warren

Carbon Copies Ltd
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Looks awesome.  Wouldn't want to ground it out though.  Made mine in the flexible resin for this very reason.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Cheers FLD. All part of the cunning plan, if they brake it they will have to buy another one.Wink

How's the rear wing coming along?

Carbon Copies Ltd
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
A cunning plan indeed!

The mould for the main element is done, just needs release agent on it.  Need to do the second element now.
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A nice carbon splitter is a good way to discourage people from excessive lowering of thier cars and driving too close to kerbs when parking end on.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Warren (Staff) (11/06/2014)
A nice carbon splitter is a good way to discourage people from excessive lowering of thier cars and driving too close to kerbs when parking end on.


SmileSmileSmile


The other Warren

Carbon Copies Ltd
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Was this a two piece mold? Did you make this similar to the bonnet hood instructional videos?

The reason I ask is I'm planning to make a large flat splitter soon. It has a beveled, leading edge in the design and I'm thinking I need to make a mold of the top AND bottom? It will be constructed around divinylcell. Any pointers would be greatly appreciated.

Thanks!
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
That ^ depends on the shape of the part. If you've got a rolled edge of the front of the part but no mechanical locks on the back then you can do it in one piece.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
BlackNDecker (15/06/2014)
Was this a two piece mold? Did you make this similar to the bonnet hood instructional videos?

The reason I ask is I'm planning to make a large flat splitter soon. It has a beveled, leading edge in the design and I'm thinking I need to make a mold of the top AND bottom? It will be constructed around divinylcell. Any pointers would be greatly appreciated.

Thanks!



Hi, I normally do splitters like this it one hit but in this case the customer wanted a gloss finish on both top and bottom. A peel ply finish on the bottom is normally acceptable to most people.

I infused the top section and removed the peel ply but left the part in the mould. At the same time I infused some flat sheet. This was then trimmed slightly over size. 10mm closed cell foam was then cut to fit tightly inside the top section, epoxy adhesive applied to both surfaces, the flat sheet positioned on top and the whole thing re bagged and left to cure under vacuum. once cured the bottom sheet was trimmed flush with top using a router and a bearing guided cutter.
Hope that helps.

Warren

Carbon Copies Ltd
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Warren,

Kind thanks for the helpful reply!

As I plan out my splitter mold, I am concerned about the gap that will develop between the beveled edge of the mold and the vertical edgle of the divinycel.


And a pic of the "plug" for the splitter mold:

Edited 11 Years Ago by BlackNDecker