Group: Forum Members
Posts: 688,
Visits: 5.4K
|
The Fiesta St I have been making parts for doesn't have a splitter as standard, this one I made should be fitted to the car pretty soon. Lay up was GC 50 - 2 x 450 CF - 10mm foam core - 2 x 450 CF using infusion.
Warren
Carbon Copies Ltd
|